It is what I've used on the last 15+ stocks for bedding.
Has anyone ever used Devcon syringe carded to as bedding compound?
https://www.amazon.com/DEVCON-Plastic-Steel-syringe-carded/dp/B01JFD42RO/ref=sr_1_5?ie=UTF8&qid=1532049073&sr=8-5&keywords=devcon+plastic+steel
I can get this at my local hardware store
It is what I've used on the last 15+ stocks for bedding.
Works better than JB Weld IMO
Not as runny as Accuglass. Let it set for 10 to 20 minutes after mixing will thicken it up. Easy to clean up excess with vinegar and Q-tips. I use acetone and Q-tips.