I have several new cans of Alum-Hyde II on hand I hate to waste...I know there are better products out there now but these are just sitting there and are the colors I want to use so....I have a stainless recoil lug...never painted SS...will scuffing it up good with a 3M sanding pad (about 300 grit) be OK for good adhesion? It did a great job of removing the Bluing-Parkerization on the 110FP barrel and action, just seems like the SS is slicker and worried about paint flaking off...I plan on baking it for overnight at 200-225 after initial cure.